Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 53.8 MPa @Temperature 23.9 °C |
7800 psi @Temperature 75.0 °F |
Short-Beam, Dry; ASTM D2344 |
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 7581 E-Glass Reinforced Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f.. |