Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 35.4 MPa | 5140 psi | Etched Aluminum Overlap, Water Vapor 66°C, 80% RH for 14 days |
3M Scotch-Weld™ DP405 LH Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel.. |