Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 5.24 MPa | 760 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR III 5/32-5052-.0025 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 5.24 MPa | 760 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR III 5/32-5056-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | >= 5.24 MPa | >= 760 psi | Plate Shear, L Direction, min, preliminary |
Hexcel® HexWeb® CR III 1/16-5056-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 5.24 MPa | 760 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR-PAA™ 5/32-5056-0.002 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | 5.24 MPa | 760 psi | Overlap, Aluminum, RT cure for 5 hrs; ASTM D1002 |
3M Scotch-Weld™ DP920 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i.. |
|||
Shear Strength | 5.24 MPa @Temperature 82.0 °C, Time 3.46e+6 sec |
760 psi @Temperature 180 °F, Time 960 hour |
Overlap, Cured for 7 days at 24°C |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |