Mechanical Properties Metric English Comments
Shear Strength 0.03597 - 0.677 MPa

@Temperature 250 - 280 °C
5.217 - 98.2 psi

@Temperature 482 - 536 °F
Average value: 0.280 MPa Grade Count:1
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Shear Strength 0.03597 - 0.677 MPa

@Shear Rate 50.0 - 5000 1/s
5.217 - 98.2 psi

@Shear Rate 50.0 - 5000 1/s
Average value: 0.280 MPa Grade Count:1
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..