Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 31.7 MPa | 4600 psi | |
Indium Corp. Indalloy 130 Tin-Lead Solder Alloy Inexpensive utility solderInformation Provided by Indium Corporation |
|||
Shear Strength | 31.7 MPa | 4600 psi | Overlap, Methyl Ethyl Ketone immersion, RT for 30 days |
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Shear Strength | 31.7 MPa | 4600 psi | Overlap, Aluminum, RT cure for 24 hrs; ASTM D1002 |
3M Scotch-Weld™ DP920 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i.. |
|||
Shear Strength | 31.7 MPa | 4600 psi | Overlap, Aluminum, 49°C for 2 hrs; ASTM D1002 |
3M Scotch-Weld™ DP920 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i.. |
|||
Shear Strength | 31.7 MPa @Temperature 81.0 - 83.0 °C |
4600 psi @Temperature 178 - 181 °F |
Average |
3M Scotch-Weld™ EC-1386 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M |
|||
Shear Strength | 31.7 MPa | 4600 psi | Aluminum, etched, Overlap, 30 day water soak, Cohesive Failure |
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives 3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f.. |
|||
Shear Strength | 31.7 MPa | 4600 psi | Aluminum, etched, Overlap, 30 day water soak, Cohesive Failure |
3M Scotch-Weld™ LSB60NS Toughened Epoxy Adhesives 3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60NS is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of.. |