Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 310 MPa @Temperature 20.0 °C |
>= 45000 psi @Temperature 68.0 °F |
Cross Breaking Strength |
Advanced Ceramics ACL 1091 (C-799) Alumina Information provided by Advanced Ceramics Limited (ACL) |