Shear Strength 2.98 MPa
432 psi
ASTM C273
3M Balsa Panels
3M™ Balsa Panels are made of end grain balsa, a highly processed ultra light wood product, imparts impressive strength and stiffness to the sandwich panel. The end grain confiation of balsa provide..