Mechanical Properties Metric English Comments
Shear Strength >= 0.300 MPa
>= 43.5 psi
ASTM C273
Parabeam Industrie Paraglass 8 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl..
Shear Strength 0.300 MPa
43.5 psi
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Shear Strength 0.300 MPa
43.5 psi
Allowable
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Shear Strength 0.300 MPa
43.5 psi
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Shear Strength 0.300 MPa
43.5 psi
Allowable
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Shear Strength 0.300 MPa
43.5 psi
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Shear Strength 0.300 MPa
43.5 psi
Allowable
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Shear Strength 0.300 MPa
43.5 psi
Allowable
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Shear Strength 0.300 MPa
43.5 psi
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Shear Strength 0.300 MPa
43.5 psi
Allowable
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Shear Strength 0.300 MPa
43.5 psi
Typical; ASTM C273
Parabeam Industrie Paraglass 10 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl..