Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 24.1 - 26.9 MPa | 3500 - 3900 psi | |
ND Industries 388 Toughened Instant Superglue Black toughened Cyanoacrylate for metal, rubber, and plastic |
|||
Shear Strength | 24.1 - 26.9 MPa | 3500 - 3900 psi | |
ND Industries Toughened Ethyl SuperGlue 310 Black flexible Cyanoacrylate for metal, rubber, and plastic |