Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 2.59 MPa
375 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 5/32-5052-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 2.59 MPa
375 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR-PAA™ 3/16-5052-0.0025 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 2.59 MPa
375 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR-PAA™ 5/32-5052-0.002 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 2.59 MPa
375 psi
Overlap, Etched Aluminum tested after 1 week of Immersion in Toulene
3M Scotch-Weld™ DP812 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP812 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Shear Strength 2.59 MPa
375 psi
On Douglas Fir
3M Scotch-Weld™ 3738 Hot Melt Adhesive
High delivery rate and long bonding rage and General purpose for foundry san cores, wood bonding, corrugated, selected plastics and chipboardInformation provided by 3M
Shear Strength 2.59 MPa
375 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 3/16-5052-.0025 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..