Mechanical Properties Metric English Comments
Shear Strength 37.2 MPa
5400 psi
Overlap, Skydrol LD-4 immersion, 66°C for 30 days
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M