Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 23.2 MPa | 3360 psi | Overlap, Aluminum-etched, with KTLN Deep Draw Lue Oil, Cohesive failure; ASTM D1002 |
3M Scotch-Weld™ DP920 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i.. |