Mechanical Properties Metric English Comments
Shear Strength 33.3 MPa
4830 psi
Etched Aluminum Overlap, Salt Spray @ 35°C for 90 days
3M Scotch-Weld™ EC-2086 Structural Adhesive
3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.Information provided by 3M