Polymer Property : Shear Strength = 32100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 221 MPa
32100 psi
Alcoa Toolrite 2011®-T3 Aluminum
Weldability = D; Stress Corrosion Cracking Resistance = D; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting ..
Shear Strength 221 MPa
32100 psi
Calculated
Aleris Alustar Aluminum Alloy, H321/H116; 2 - 20 mm thickness
At least 20% stronger than AA 5083 before and after welding. Bendability and weldability similar to AA 5083. High corrosion resistance. Provides options for ship design and building.Composition d..
Copyright © lookpolymers.com All Rights Reserved