Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 2.20 MPa | 319 psi | ASTM C273 |
3A Composites Core Materials AIREX® PXw.420 Fiber-Reinforced Structural Foam Panel AIREX® PXw is a closed-cell, fiber reinforced polymer foam panel with a special formulation and very high mechanical properties. The sophisticated manufacturing process evenly distributes continuou.. |