Polymer Property : Shear Strength = 31200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 215 - 265 MPa
31200 - 38400 psi
Goodfellow Potassium Aluminosilicate (Muscovite Mica)
Mica is a naturally occurring mineral and as such its exact composition varies between grades, as will its properties. Ruby Mica is the highest grade of Muscovite Mica. The name comes from the Latin..
Shear Strength 215 MPa
31200 psi
Calculated
Aleris Alustar Aluminum Alloy, H321/H116; 20 - 40 mm thickness
At least 20% stronger than AA 5083 before and after welding. Bendability and weldability similar to AA 5083. High corrosion resistance. Provides options for ship design and building.Composition d..