Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 21.1 MPa | >= 3060 psi | Die |
Epoxy Technology EPO-TEK® EJ2189 Electrically Conductive Epoxy Product Description: EPO-TEK® EJ2189 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although othe.. |