Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 207 MPa
30000 psi
Ultimate
Kaiser 6040 T8 Rod & Bar
6040 is a lead-free alternative to 6262. The alloy offers very good machinability along with good corrosion resistance. It also has excellent coating acceptance (anodize response). It can be used in..
Shear Strength 207 MPa
30000 psi
Meehanite GE-30 Flake Graphite Cast Iron
Type GE-30 combines improved strength and solidity with higher machining feeds and speeds than ordinary gray iron.General Meehanite information - Meehanite metal is first melted to a definite degree..
Shear Strength 207 MPa
30000 psi
Alcoa Toolrite 2011®-T4 Aluminum
Weldability = D; Stress Corrosion Cracking Resistance = D; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting ..
Shear Strength 207 MPa
30000 psi
Dura-Bar G1 Continuously Cast Gray Iron Bar Stock ASTM A48
Dura-Bar G1 contains flake graphite in a matrix that is pearlitic with small amounts of ferrite. This is the softest grade of the Dura-Bar gray irons and is normally selected when excellent machinab..
Shear Strength 207 MPa
30000 psi
Dura-Bar G2A Continuously Cast Gray Iron Bar Stock ASTM A48
Dura-Bar G2A has Type D graphite in a predominantly pearlitic matrix. The fine graphite structure allows excellent surface finish and is normally used in permanent mold applications requiring optima..