Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 3.88 MPa | 563 psi | |
Valley Adhesives EM-110 High Performance Application Glue Stick Valley Adhesives EM-110 High Performance Application Glue StickHigh peel, shear strength, and heat resistance; Good wetting and heat resistance for potting; Excellent adhesion to wood, plastics, pol.. |
|||
Shear Strength | 3.88 MPa | 563 psi | |
Valley Adhesives EM-422 High Temperature Application Glue Stick Valley Adhesives EM-422 High Temperature Application Glue StickRapid strength build up; Excellent hot tacking and wetting; Bonds corrugated boxes and paper in packaging operations and repackaging ar.. |