Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 3.20 MPa | >= 464 psi | ISO 1922 |
3A Composites Core Materials AIREX® C70.200 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negli.. |