Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 19.07 MPa | 2766 psi | after 7 days Immersion in JP-4 Fuel |
3M Scotch-Weld™ EC-1469 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1469 is a one-part, 100% solids, thermosetting liquidInformation provided by 3M |
|||
Shear Strength | 19.07 MPa | 2766 psi | after 7 days Immersion in Anti-icing Fluid |
3M Scotch-Weld™ EC-1469 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1469 is a one-part, 100% solids, thermosetting liquidInformation provided by 3M |