Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 27.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 27.9 MPa
4050 psi
Overlap, Stainless Steel, Adhesive Failure
3M Scotch-Weld™ DP807 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP807 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Shear Strength 27.9 MPa
4050 psi
Overlap, Diesel Fuel for 14 days, Cohesive Failure
3M Scotch-Weld™ DP810NS Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 27.9 MPa
4050 psi
Overlap, Aluminum - bare, Adhesive Failure
3M Scotch-Weld™ DP812 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP812 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Copyright © lookpolymers.com All Rights Reserved