Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1.79 MPa | 260 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-10 - 1/8- 8.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | 1.79 MPa | 260 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRP - 1/4 - 3.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | >= 1.79 MPa | >= 260 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® HRP - 1/4 - 6.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | >= 1.79 MPa | >= 260 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® HRP - 3/8 - 4.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | 1.79 MPa | 260 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRP/OX - 1/4 - 4.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | 1.79 MPa | 260 psi | Overlap, Mahogany, 50% RH |
3M 4200 Marine Adhesive/Sealant Fast Cure A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds to wood, gelcoat and fiberglass. It forms watertight, weather-resistant seals on joints an.. |
|||
Shear Strength | 1.79 MPa | 260 psi | Overlap, Glass, Borosilicate |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |