Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 26.88 MPa | 3898 psi | Overlap on Anodized Aluminum |
3M Scotch-Weld™ EC-1386 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M |