Shear Strength 25.6 MPa
3710 psi
Tensile
Resin Technology Group Fusion 519 Wicking Grade Fusion Cyanoacrylate
Information provided by Resin Technology Group.
Shear Strength 25.6 MPa
3710 psi
Tensile
Resin Technology Group Fusion 60 Low Odor, Low Bloom Fusion Cyanoacrylate
Information provided by Resin Technology Group.