Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1.70 MPa | 247 psi | average; ISO 1922 |
3A Composites Core Materials AIREX® C70.90 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Shear Strength | 1.70 - 31.0 MPa @Temperature -55.0 - 177 °C |
247 - 4500 psi @Temperature -67.0 - 351 °F |
Average value: 14.2 MPa Grade Count:5 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |