Mechanical Properties Metric English Comments
Shear Strength 239 MPa
34700 psi
Calculated
Alcoa Excalibar® 6013-T8 Aluminum, 1.9-3.8 cm diameter
Weldability = A; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6013 characteristics and uses: High strength and good corrosion resistance...