Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.110 - 16.0 MPa | 16.0 - 2320 psi | Average value: 3.10 MPa Grade Count:16 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |