Polymer Property : Shear Strength = 2125 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 14.65 MPa
2125 psi
Overlap, Etched Aluminum tested after 1 week of Immersion in 66°C tap water
3M Scotch-Weld™ DP812 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP812 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Shear Strength 14.65 MPa
2125 psi
Overlap, Etched Aluminum
3M Scotch-Weld™ DP812 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP812 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..