Mechanical Properties Metric English Comments
Shear Strength 21.7 MPa
3150 psi
Overlap, Etched Aluminum tested after 1 week of Immersion in 66°C and 80% RH
3M Scotch-Weld™ DP807 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP807 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Shear Strength 21.7 MPa
3150 psi
Overlap, Gasoline for 14 days, Cohesive Failure
3M Scotch-Weld™ DP810NS Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 21.7 MPa

@Temperature -55.0 °C,
Time Error in fixSigDigits: @digits must be between 1 a sec
3150 psi

@Temperature -67.0 °F,
Time Error in fixSigDigits: @digits must be between 1 a hour
3M Scotch-Weld™ EC-1469 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive EC-1469 is a one-part, 100% solids, thermosetting liquidInformation provided by 3M
Shear Strength 21.7 MPa
3150 psi
Overlap, IPA for 14 days, Cohesive Failure
3M Scotch-Weld™ DP810 Tan Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 21.7 MPa

@Temperature 23.0 °C
3150 psi

@Temperature 73.4 °F
Overlap, Etched Alum/Etched Alum
3M Scotch-Weld™ DP820 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..