Polymer Property : Shear Strength = 21.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 21.5 MPa
3120 psi
Bond, Al to Al, after 30 days water absorption
Master Bond EP30P Epoxy Bonds Glass, Polycarbonates and Acrylics
Description: Master Bond Polymer Adhesive EP30P is a two component, transparent, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is for..
Shear Strength >= 21.5 MPa
>= 3120 psi
Bond, Al to Al, after 30 days water absorption
Master Bond EP30LV Optically Clear, Low Viscosity Epoxy Adhesive
Description: Master Bond Polymer System EP30LV is a low viscosity, two component epoxy adhesive for general purpose bonding, coating, sealing and casting formulated to cure at room temperature or mo..
Shear Strength 21.5 MPa
3120 psi
Overlap, Etched Al, Tap water at RT for 14 days
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..
Shear Strength 21.5 MPa

@Temperature -53.0 °C,
Time 0.000 sec
3120 psi

@Temperature -63.4 °F,
Time 0.000 hour
Overlap, Cured for 7 days at 24°C
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..