Shear Strength 2.34 MPa
340 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 1/4-5052-.003 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 2.34 MPa
340 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR III 1/8-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 2.34 MPa
340 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 1/8-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength >= 2.34 MPa
>= 340 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® CR III 3/16-5056-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 2.34 MPa
340 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR-PAA™ 1/8-5052-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 2.34 MPa
340 psi
Plate Shear, W Direction, typ, preliminary value obtained at .500 inch thickness
Hexcel® HexWeb® HRH-327 - 3/8 - 7.0 Fiberglass Reinforced Polyimide Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a..
Shear Strength 2.34 MPa
340 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR-PAA™ 1/8-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength >= 2.34 MPa
>= 340 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® CR-PAA™ 3/16-5056-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength >= 2.34 MPa
>= 340 psi
Die
Epoxy Technology EPO-TEK® 301 Spectrally Transparent Epoxy
Product Description: EPO-TEK® 301 is a two component, room temperature curing epoxy featuring very low viscosity, and excellent optical-mechanical properties.Advantages & Application Notes: Semicon..
Shear Strength >= 2.34 MPa
>= 340 psi
Die
Epoxy Technology EPO-TEK® T7109-18 Electrically Insulating Epoxy Paste
Material Description: A flexible, electrically insulating epoxy paste designed for low stress and heat dissipation applications. Alternative to EPO-TEK® T7109-17.Information Provided by Epoxy Tec..
Shear Strength 2.34 MPa
340 psi
Lap Shear Strength; ASTM D1002
Arlon Thermabond® T-20 NP (99770W008) 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: 8 mil Primerless Thermabond®. T-20 NP. Thermally conductive, electrically insulating electronic adhesive. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Ru..
Shear Strength 2.34 MPa
340 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.003 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..