Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 6.76 - 137 MPa | 980 - 19900 psi | Average value: 78.6 MPa Grade Count:51 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |