Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 26.2 - 124 MPa @Temperature -55.0 - 177 °C |
3800 - 18000 psi @Temperature -67.0 - 351 °F |
Average value: 57.4 MPa Grade Count:22 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |