Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 18.1 MPa @Temperature 316 °C |
2620 psi @Temperature 601 °F |
Etched Aluminum Overlap, 2 min cure |
3M Scotch-Weld™ EC-1386 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M |