Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 119 MPa | 17300 psi | ASTM C273 |
SABIC Innovative Plastics LNP THERMOCOMP LC006EXQ PEEK LNP* THERMOCOMP* LC006EXQ is a compound based on Polyetheretherketone containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding. |