Mechanical Properties Metric English Comments
Shear Strength 17.1 MPa
2480 psi
Overlap, Galvanized Steel Okite degrease Hot dip
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..