Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 159 MPa @Thickness 15.7 mm |
23000 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP130HF Glass Fabric Description: High flexural, impact and tensile strength glass fabric epoxy laminate, especially in the machine direction. Engineered to provide better physical properties than NEMA FR-4. More dimens.. |
|||
Shear Strength | >= 159 MPa | >= 23000 psi | Bond, Al to Al |
Master Bond EP45HTQ Quartz Filled Heat Resistant Epoxy Description: Master Bond Polymer Compound EP45HTQ is a two component quartz filled, epoxy compound for high performance structural bonding and casting. It is suitable for applications where long ter.. |
|||
Shear Strength | 159 MPa | 23100 psi | Calculated |
Alcoa UltrAlloy® 6020-T651 Aluminum Weldability = B; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6020 characteristics and uses: Excellent machinability, high corrosion resi.. |