Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 15.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 15.5 MPa
2250 psi
CRS Overlap, Hydraulic Oil at RT
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir..
Shear Strength 15.5 MPa
2250 psi
CRS Overlap, Tap Water at RT
3M Scotch-Weld™ 183 B/A Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flowable product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent e..
Shear Strength 15.5 MPa
2250 psi
Overlap, Etched Aluminum tested after 1 week of Immersion in 66°C tap water
3M Scotch-Weld™ DP807 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP807 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Shear Strength 15.5 MPa
2250 psi
Overlap at 1 hr after bonding
3M Scotch-Weld™ DP810 Tan Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 15.5 MPa

@Time 1800 sec
2250 psi

@Time 0.500 hour
Aluminum Overlap
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Copyright © lookpolymers.com All Rights Reserved