Polymer Property : Shear Strength = 15.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 15.3 MPa
2220 psi
Overlap, PVC, Substrate Failure
3M Scotch-Weld™ DP8010 Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl..
Shear Strength 15.3 MPa
2220 psi
Overlap, Etched Aluminum, Water soak at RT-Cohesive Failure; ASTM D1002
3M Scotch-Weld™ LSB90 Flexible Epoxy
3M™ Scotch-Weld™ Epoxy Adhesive LSB90 is a high performance, two-part, flexible epoxy adhesive offering high shear and peel adhesion and very high levels of durability. It has a 90 minute worklife..