Shear Strength 15.22 MPa

@Temperature 260 °C
2208 psi

@Temperature 500 °F
Etched Aluminum Overlap, 10 min cure
3M Scotch-Weld™ EC-1386 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M