Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 148.6 MPa | 21550 psi | |
Meehanite GF-20 Flake Graphite Cast Iron Type GF-20 is designed principally for high machinability and is used where ultimate strength is not an important factor.General Meehanite information - Meehanite metal is first melted to a definite.. |