Polymer Property : Shear Strength = 1456 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 10.04 MPa
1456 psi
Lap
Epoxy Technology EPO-TEK® 377 High Temperature Epoxy
Product Description: EPO TEK®377 is a two component, high Tg, fiber optic grade epoxy adhesive. It is well suited for semiconductor, medical and optical applications.Advantages & Application Notes:..