Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 6.89 - 14.8 MPa | 1000 - 2150 psi | Lap; ASTM D1002 |
3M Scotch-Weld™ RT41 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |