Polymer Property : Shear Strength = 1390 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 9.58 MPa

@Temperature 81.0 - 83.0 °C
1390 psi

@Temperature 178 - 181 °F
Etched Aluminum Overlap, 1.2% (Radiator Conditioner) 98.9% Tap Water Immersion for 30 days
3M Scotch-Weld™ EC-1386 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M
Shear Strength 9.58 MPa
1390 psi
Overlap, Etched Al, 100% RH at 49°C for 30 days
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..