Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.883 MPa | 128 psi | Plate Shear, L Direction, typical value |
Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 2.5 Aramid Honeycomb Designation: Material-Cell Size (cells per lineal foot in W direction)-Density (lb per cubic foot)HexWeb HRH-36 Flex-Core aramid paper is reinforced with a high temperature phenolic resin. This prod.. |
|||
Shear Strength | 0.883 MPa | 128 psi | Plate Shear, W Direction, typical value |
Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 3.5 Aramid Honeycomb Designation: Material-Cell Size (cells per lineal foot in W direction)-Density (lb per cubic foot)HexWeb HRH-36 Flex-Core aramid paper is reinforced with a high temperature phenolic resin. This prod.. |