Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 86.9 MPa | 12600 psi | ASTM D732 |
Quadrant EPP Semitron® ESd 520HR (ASTM Product Data Sheet) |
|||
Shear Strength | 86.9 MPa | 12600 psi | Short Beam |
Hexcel® HexPly® EH04 Epoxy Resin System, Fortafil 510 Fiber F510 150 24" EH04 38%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel |