Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 8.69 MPa | 1260 psi | Cured, tensile |
Resin Technology Group UV MX-2230 Quick Fixture, Activator Cured, One-Component, Acrylic Adhesive UV MX 2230 is a one-component acrylate based polymer designed to be used as a quick-fixture, surface activated adhesive, (with optional UV or oven cure), for applications on a variety of substrates .. |
|||
Shear Strength | 8.69 MPa | 1260 psi | Overlap, Etched Al, Salt Spray at RT for 30 days |
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 8.69 MPa @Temperature 82.0 °C, Time 900 sec |
1260 psi @Temperature 180 °F, Time 0.250 hour |
Aluminum Overlap |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |