Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 123 MPa | 17900 psi | ASTM D732 |
Haysite EMD Polyester, Glass Reinforced EMD is a glass mat reinforced polyester sheet designed primarily as a "slot wedge" material in large motors and generators. EMD has low weight loss at elevated temperatures and high flexural and sh.. |