Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 70.0 - 84.0 MPa | 10200 - 12200 psi | IS 867-1963 |
Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium/hard flow Applications: Elec.. |
|||
Shear Strength | 70.0 - 84.0 MPa | 10200 - 12200 psi | IS 867-1963 |
Amity Thermosets ATO 145 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium flow Applications: Electric .. |